Study on properties of W-Ni-Fe alloy for high speed precision cutting by PCBN tool |
ZHANG Yan,XIA Zhi-hui,XU Dong-ming |
Institute of Machinery Manufacturing Technology, Chinese Academy of Engineering Physics, Mianyang 621900, China |
|
|
Abstract The high-speed precision cutting experiment was conducted on W-Ni-Fe alloy using PCBN cutting tool. The failure and wear mechanism were analyzed by observing the rake and flank face of the cutting tool. Meanwhile, the cutting performance of PCBN tool when cutting W-Ni-Fe alloy was studied from the aspects of CBN contents, tool parameters and surface roughness. Results show that, the PCBN tool with high CBN content and large tip radius presents a longer life, and good surface quality is obtained in the condition of high cutting speed, low feeding rate and low cutting depth. The wear mechanism of W-Ni-Fe alloy in high speed precision cutting of PCBN tool is mainly composed of adhesive wear, diffusion wear, local peeling, oxidation wear, chipping wear and multiple results of them.
|
Received: 26 November 2015
Published: 15 December 2016
|
|
|
|
[1] 陈永杰,王海阔等. 聚晶立方氮化硼的制备方法及应用进展[J]. 金刚石与磨料磨具工程,2005,35(206).
[2] 刘献礼. 聚晶立方氮化硼刀具及其应用[M]. 哈尔滨: 黑龙江科学技术出版社, 1999.
[3] 计伟,刘献礼等. PCBN刀具切削GH706磨损特征研究[J]. 摩擦学学报,2015,1(35):37-44.
[4] 王发展,唐丽霞等. 钨材料及其加工[M].北京:冶金工业出版社,2008.
[5] Ma Y Z, Zhang J J, Liu W S. Transient Liquid-Phase Sintering Characteristic of W-Ni-Fe Alloy via Microwave-Assisted Heating [J]. Rare Metal Materials and Engineering, 2014, 43: 2108–2111
[6] 刘文胜,唐芳,马运柱. 微量Cr 对93W-Ni-Fe 合金组织及力学性能的影响[J].中国有色金属学报,2008,18(9):1645-1650.
[7] 王伏生,赵慕岳. 高密度钨合金及其在军事工业中的应用[J].粉末冶金材料科学与工程,1997(2):114-119.
[8] 叶伟昌,梁萍. 钨及其合金的切削加工[J].硬质合金,2004, 21(1):52-55.
[9] 刘战强, 万熠. PCBN 刀具磨损形态与磨损规律的实验研究[J].农业机械学报,2004(5).
[10] Lopezdelacalle L N, Perez J, Llorente J I, Sanchez J A. Advanced cutting conditions for the milling of aeronautical alloys [J]. Journal of Materials Processing Technology, 2000, 100: 1–11.
[11] 李启泉,张旺玺等. 不同PCBN刀具车削硼铸铁的对比研究[J].金刚石与磨料磨具工程,2015,35(206):63-68.
|
|
|
|